Vanadium oxide films
+1-480-493-0093

Vanadium oxide films

MDT-file: Download
Film of vanadium oxide on glass surface.
Vanadium sputtered on glass with the subsequent oxidation in natural conditions. Annealing of the sample was carried out at 500 оС during 10 min in dry oxygen.
Image courtesy of Gusev E.Yu., Taganrog State University Of Radioengineering.
The sample was kindly given by Dzhuplin V.N., Ageev O.A., Taganrog State University Of Radioengineering.

d_vanadium_4
d_vanadium_4
Vanadium films

Film of vanadium oxide on glass surface.
Vanadium sputtered on glass with the subsequent oxidation in natural conditions. Annealing of the sample was carried out at 500 оС during 10 min in dry oxygen.

Image courtesy of Gusev E.Yu., Taganrog State University Of Radioengineering.
The sample was kindly given by Dzhuplin V.N., Ageev O.A., Taganrog State University Of Radioengineering.


size: 2x2 um
SPM principle: Intermittent contact mode